Skip to content
Burhan Enterprises logoBURHAN ENTERPRISESComplex Fabric Solutions
← Insights
Sourcing Practice25 November 2026· 8 min read

Colour Fastness Grades Explained: What 3–4, 4 and 4–5 Mean on a Report

Colour fastness grade 4 meaning explained: how grey scales rate shade change and staining, how half grades work, and how to set pass grades on a report.

Colour Fastness Grades Explained: What 3–4, 4 and 4–5 Mean on a Report — article cover image

The colour fastness grade 4 meaning is simple: the test caused a small but visible difference, judged equal to the grade 4 pair on an ISO grey scale. The scale runs from 5, no perceived difference, down to 1, the largest. Whether 4 passes depends on the threshold in your specification.

What does colour fastness grade 4 mean?

A colour fastness grade is a visual rating of how much a test changed or transferred colour. The assessor places tested and untested cloth side by side and compares that contrast with pairs of reference chips. Grade 4 means the contrast looks like the grade 4 pair.

Grade 5 is given only when no difference is perceived.

Three things the grade does not tell you:

  • Shade accuracy. A fabric can grade 5 for fastness and still miss the colour target. That target is set by the approved lab dip.
  • Repeat consistency. Two lots can both grade 4 and differ visibly from each other, which is a separate question when reordering the same fabric.
  • Light fastness. Light is commonly rated against blue wool references on a separate 1 to 8 scale, so a 4 there is a different measure.

How do the grey scales for colour change and staining differ?

The ISO 105-A02 scale rates change in colour: how far the tested specimen has moved from the untested original. The ISO 105-A03 scale rates staining: how much colour has transferred onto an undyed adjacent cloth. A02 pairs a neutral grey chip with a lighter grey one; A03 pairs a white chip with a darker one.

The same number therefore covers different amounts of colour difference. These are the nominal CIELAB differences the two standards specify for the chip pairs, each with its own tolerance:

GradeChange in colour scale (CIELAB)Staining scale (CIELAB)
500
4–50.82.2
41.74.3
3–42.56.0
33.48.5
2–34.812.0
26.816.9
1–29.624.0
113.634.1

The steps are not even: from grade 4 downwards, each whole grade roughly doubles the colour difference, so moving from 3 to 2 is about twice the drop of moving from 4 to 3. And grade 4 for staining allows about 2.5 times the CIELAB difference of grade 4 for colour change (4.3 ÷ 1.7), so never treat the two columns as interchangeable.

What do half grades such as 3–4 and 4–5 mean?

A half grade is a rating between two whole grades. The essential scale has five pairs, and an assessor using it gives 4–5 when the contrast looks nearer the imagined midpoint between 4 and 5 than either pair. The nine-step scale adds physical pairs for 4–5, 3–4, 2–3 and 1–2, and the assessor picks the nearest.

Read a half grade as a scale position, not a decimal:

  • 3–4 sits below 4. If your line says "grade 4 or better", a 3–4 fails it.
  • 4–5 sits above 4. It meets the same line.
  • The notation varies. ISO writes 4-5, while AATCC gray scale material writes 4.5 for the same step. Neither is an arithmetic value.

For change in colour, a report can also add a qualifier after the number, such as 3 weaker or 4-5 redder, because the grade rates overall contrast and not the character of the change. ISO 105-A02 makes these words optional, so ask for them on any line near your limit.

Do not average grades across shades or bands. They are ordered steps on an uneven scale, and an average can hide the one result that fails.

Why does a report list several staining grades for one test?

A wash test commonly places your fabric against a multifibre adjacent fabric, a strip woven with bands of different fibres, because dye that releases in the wash does not stain every fibre equally. The report shows one change-in-colour grade plus one staining grade per band.

ISO 105-F10 specifies two six-fibre strips. DW carries secondary acetate, bleached cotton, polyamide, polyester, acrylic and wool. TV replaces acetate and wool with triacetate and viscose, for test procedures that cannot run with those fibres present. The report should state which adjacent fabric was used.

BandWhat a low grade warns you about
Acetate or triacetateMarking on acetate linings. Commonly sensitive to disperse dye
Bleached cottonBleed onto white cotton trims, pocketing and contrast panels
PolyamideMarking on nylon linings and stretch trims. Also commonly picks up disperse dye
PolyesterMarking on polyester panels and blends
AcrylicMarking on acrylic knit trims
Wool or viscoseMarking on wool blends or viscose linings

On a polyester-cotton blend, low acetate and polyamide grades often point towards the polyester-side disperse dye, and a low cotton grade more likely points towards the cotton side. Set one threshold for every band by default, because garments are washed in mixed loads. Exempt a band only by written agreement, and accept that the risk then moves to you.

Why do wet rubbing grades usually come out lower than dry?

A rubbing test, also called crocking, moves a white cloth across the fabric under load and rates the mark left on that cloth with the staining scale. ISO 105-X12 allows one test with a dry cloth and one with a wet cloth, so the report shows a dry and a wet grade and no change-in-colour grade.

Wet usually grades lower because water mobilises dye that is not fixed to the fibre. On reactive-dyed cotton that is hydrolysed and unreacted dye left after dyeing, so the first remedy is thorough washing-off and soaping. Deep shades carry more of this loose material, so a deep navy cotton twill is usually a harder case than a pale cotton lawn.

  • The trade-off. Wet rubbing improvers can lift a result, but published results vary with depth of shade and they add a chemical step. Test the finished cloth.
  • The method matters. ISO 105-X12 soaks the wet cloth to a take-up of 95% to 100%, while AATCC TM8 is generally run at about 65%. An ISO wet grade and an AATCC wet grade are therefore not directly comparable.
  • The soak level matters too. ISO 105-X12 notes that soak can dramatically affect ratings, cites 65 ± 5% as a commonly used level and requires the report to state the percentage. Name one method and one soak level.

How should a pass grade be written into a fabric specification?

Write each threshold as a minimum per test, per scale and per shade, agreed for the programme. No universal pass grade fits every end use, so the brackets below are placeholders. Use the pre-bulk testing checklist to decide which tests to order, then write the lines like this:

  • Wash method: ISO 105-C06, test condition [named], on production-intent fabric
  • Change in colour: grade [X] or better on the ISO 105-A02 scale
  • Staining: grade [X] or better on every band of the [DW or TV] strip, on the ISO 105-A03 scale
  • Rubbing: ISO 105-X12, wet soak [named], dry grade [X] or better, wet grade [Y] or better
  • Shades covered: every colourway, or named shades only
  • Lab route: who tests, and whose result governs, since visual grades near a limit can differ
  • Failure: retest, re-finish or rejection before cutting

Two decisions belong on the order:

  • A separate wet grade for deep shades. One wet figure across a range may be easy for pastels and hard for navy or black. The cost is an explicit lower standard on those colours.
  • Which shades to test. Testing only the deepest shade saves lab time, but a bright colour on a different dye can fail where black passes.

Burhan Enterprises is a Karachi sourcing partner, not a mill: we match a requirement to suitable partner units and hold the specification and approvals through production. To put fastness lines on a new programme, look at dyed fabric qualities or start through custom development.

Quick answers

Is colour fastness grade 4 good? Grade 4 means a small but visible difference after the test, on a scale where 5 is no perceived difference and 1 is the largest. It is neither good nor bad on its own. It passes only if the buyer and supplier agreed a threshold of 4 or lower for that test, scale and shade before bulk.

Is 3–4 a pass if the specification says grade 4? No. A 3–4 is the half grade between 3 and 4, so it sits below a minimum of grade 4 and fails a line written as "grade 4 or better". A 4–5 sits above that minimum and meets it. Half grades are steps on the grey scale, not decimals, so they should not be rounded up.

Why does a fastness report show so many staining grades? A wash test is commonly run against a multifibre strip, and dye released in the wash stains each fibre differently. ISO 105-F10 strips carry six fibres, so that report gives one change-in-colour grade for the fabric and six staining grades. Read the lowest staining grade against the threshold, and check which band it came from.

Does a grey scale grade show that a fabric matches the approved shade? No. Grey scales for fastness rate how much a test changed the fabric or how much colour transferred onto adjacent cloth. They do not compare bulk with a colour target. Shade accuracy is judged against the approved lab dip or colour standard, so a fabric can have excellent fastness grades and still fail shade approval.

Ready to source this?

Free swatches, honest lead times, one accountable partner.

Request free swatches

Sourcing notes by email

By subscribing, you agree we may email you sourcing insights. Unsubscribe any time. See our Privacy Policy.

Have a fabric requirement?

Tell us what you're making — we'll help you source it.

Request SwatchesWhatsApp